Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Americas - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

UL Yellow Card Link E121562-221243
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 12 cm³/10min ISO 1133
Temperatura 260 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 14 g/10min ASTM D 1238
Temperatura 260 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 1370 MPa ISO 527
Carico unitario a trazione 35 MPa ISO 527
Deformazione a rottura 50 % ISO 527
ASTM Data
Modulo a trazione 1240 MPa ASTM D 638
Resistenza alla trazione di snervamento 35 MPa ASTM D 638
Resistenza alla trazione a rottura 34 MPa ASTM D 638
Allungamento a snervamento 8 % ASTM D 638
Allungamento a rottura 125 % ASTM D 638
Modulo a flessione 1370 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 534 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di rammollimento Vicat, A 131 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
ASTM Data
DTUL a 66 psi 112 °C ASTM D 648
DTUL a 264 psi 85 °C ASTM D 648
Temp.di rammollimento Vicat 86 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Densità 990 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 60 - 65 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 260 - 290 °C -
Temperatura dello stampo 30 - 50 °C -
Zona 1 225 - 275 °C -
Zona 2 240 - 280 °C -
Zona 3 250 - 290 °C -
Velocità di Rotazione della Vite 20 - 100 rpm -
Contropressione 0.3 - 0.7 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.